ENH:[Process/Filament] Add missing materials for model O1E Profile Edited by shsst

Change-Id: I92a543d7c5624dd93a5495c3741cb06e56c2e158
(cherry picked from commit 22e22d112a3ee4ca26637dd81f8c60abb8c98ec2)
This commit is contained in:
qian.wang
2025-08-13 14:58:47 +08:00
committed by Noisyfox
parent 20a9682c18
commit a66a1b60a8
95 changed files with 2410 additions and 197 deletions

View File

@@ -5,19 +5,6 @@
"from": "system",
"setting_id": "GFSN99_01",
"instantiation": "true",
"description": "When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.",
"chamber_temperatures": [
"60"
],
"fan_cooling_layer_time": [
"65"
],
"fan_max_speed": [
"85"
],
"fan_min_speed": [
"40"
],
"filament_deretraction_speed": [
"nil",
"nil"
@@ -114,31 +101,10 @@
"260",
"260"
],
"nozzle_temperature_range_high": [
"280"
],
"nozzle_temperature_range_low": [
"240"
],
"overhang_fan_speed": [
"95"
],
"overhang_fan_threshold": [
"10%"
],
"required_nozzle_HRC": [
"3"
],
"retraction_distances_when_ec": [
"4",
"4"
],
"slow_down_layer_time": [
"8"
],
"slow_down_min_speed": [
"10"
],
"compatible_printers": [
"Bambu Lab H2D 0.4 nozzle",
"Bambu Lab H2D 0.6 nozzle",