ENH:[Process/Filament] Add missing materials for model O1E Profile Edited by shsst

Change-Id: I92a543d7c5624dd93a5495c3741cb06e56c2e158
(cherry picked from commit 22e22d112a3ee4ca26637dd81f8c60abb8c98ec2)
This commit is contained in:
qian.wang
2025-08-13 14:58:47 +08:00
committed by Noisyfox
parent 20a9682c18
commit a66a1b60a8
95 changed files with 2410 additions and 197 deletions

View File

@@ -5,5 +5,8 @@
"from": "system",
"filament_id": "GFN06",
"instantiation": "false",
"description": "When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials."
"description": "When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.",
"impact_strength_z": [
"4.3"
]
}