Optimised for the Artillery M1 Pro printer (#12885)

* Optimised for the Artillery M1 Pro printer

* tidy up

---------

Co-authored-by: SoftFever <softfeverever@gmail.com>
This commit is contained in:
liuyingmo
2026-03-22 23:58:34 +08:00
committed by GitHub
parent 73be083ac5
commit 3d4aff5ea8
156 changed files with 3327 additions and 2374 deletions

View File

@@ -1,9 +1,9 @@
{
"from": "system",
"type": "filament",
"name": "Artillery PA-CF @Artillery M1 Pro 0.4 nozzle",
"inherits": "Artillery Generic PLA",
"from": "system",
"instantiation": "true",
"is_custom_defined": "0",
"complete_print_exhaust_fan_speed": [
"0"
],
@@ -17,16 +17,16 @@
"30"
],
"fan_min_speed": [
"30"
"10"
],
"filament_flow_ratio": [
"0.93"
],
"filament_max_volumetric_speed": [
"6"
"4"
],
"additional_cooling_fan_speed": [
"100"
"0"
],
"filament_settings_id": [
"Artillery PA-CF @Artillery M1 Pro 0.4 nozzle"
@@ -35,10 +35,10 @@
"PA-CF"
],
"nozzle_temperature": [
"250"
"280"
],
"nozzle_temperature_initial_layer": [
"250"
"280"
],
"nozzle_temperature_range_high": [
"280"
@@ -49,7 +49,6 @@
"slow_down_layer_time": [
"2"
],
"version": "2.1.2.2",
"compatible_printers": [
"Artillery M1 Pro 0.4 nozzle"
],
@@ -69,16 +68,16 @@
"0.6"
],
"temperature_vitrification": [
"108"
"170"
],
"enable_pressure_advance": [
"1"
],
"hot_plate_temp": [
"50"
"100"
],
"hot_plate_temp_initial_layer": [
"50"
"100"
],
"slow_down_min_speed": [
"10"
@@ -96,10 +95,10 @@
"100"
],
"cool_plate_temp": [
"110"
"100"
],
"cool_plate_temp_initial_layer": [
"110"
"100"
],
"overhang_fan_speed": [
"80"